Analysis Note
Raman Spectroscopic Data:ID/IG = 1.84±0.25I2D/IG = 2.12±0.322D FWHM = 41 cm-1
Application
Composites. Conductive inks. Electrodes for LiB. Energy storage & harvesting applications. Bio-medical applications.
Legal Information
Graphene Nanoribbon Composites and Methods of Making the Same, WO/2012/112435 A1.
Packaging
500 mg in glass bottle
Preparation Note
Preferred dispersing organic solvents: pyrrolidones and chlorinated solvents, also dispersible in acetone, ethyl acetate, dimethyl formamide, ethylene glycol, or 1,2-dimethoxyethane at concentration ≤0.1 mg/mL after bath sonication for 15 min with stability for a few hours. Less preferred dispersing organic solvents: cyclohexanone and γ-butyrolactone. Aqueous dispersions are possible at 0.1 mg/mL with triton-X-100, sodium cholate and deoxycholate and cellulose-based surfactants.